Organic semiconductor bilayer with full thermal treatment (BL-RT)
Arianna Quesada
ICMAB-CSIC
Laura Rodríguez
ICMAB-CSIC
Thin bilayer of organic semiconductor materials deposited on a quartz substrate, following thermal treatment of the entire bilayer for 10 minutes at 160 °C. The image was obtained using atomic force microscopy (AFM).